Customer ratings for COVERAL GR2532 Aluminium Drossing/Covering Flux-1kg

COVERAL GR2532 Aluminium Drossing/Covering Flux-1kg
$30.00
Please note: no GST
Product data sheet
Delivery weight: 1 kg

COVERAL GR2532 Aluminium Drossing/Covering Flux-1kg

Application: place COVERAL GR 2532 is spread over the melt surface after melting is complete. The flux must be stirred vigorously with the dross on the melt surface using a preheated perforated ladle until a dry dross is achieved. Once reaction is over the dross should be carefully removed using an appropriate skimming tool. 
 
Addition rate: 0.05 - 0.1 % of the metal weight depending on application type and foundry conditions.
 
Technical Data: Granulated flux Suitable for all types of Aluminium alloys with the exception of AlMg alloys Application temperature: 670 °C and higher 
 
Storage: Air tight container

In stock


Have you already had experiences with this product?

We are interested in your opinion! Tell other customers about your experiences and rate this product.
Name
Publicly visible
 
Email *
Is not published

Points *
Assign points.
 
How do you rate this product? *
 
Your experiences with this product
 
How detailed is your rating?

Important information
Your review will only be published here, and helps us to improve the quality of items we offer.
You must not use the review function to publish content that is commercial, political, pornographic, obscene, criminal, libellous or that is otherwise illegal in nature. Copying opinions that have already been published elsewhere is forbidden by law. We reserve the right not to publish reviews. You are entitled to view and correct the data collected about you and to object to it being processed. Please note our information under Privacy policy.
* Required fields
Number of ratings: 1
Average rating: 5
Works well
from albert poulis on 9/03/2021
I use a lot of aluminium that i find at scrap yards which is normally dirty so i expect a lot of dross build up and since i used coveral gr2532 i have had a better experience with moulding because i have more alloy to poor.